Papua New Guinea Pre-dispersed crosslinker TCY-70

Under normal circumstances, the pre-dispersed crosslinking agent TCY-70 can be used as an effective vulcanizing agent for halogen-containing rubber, such as CO, ECO, CIIR and BIIR, as well as a vulcanizing agent for ACM rubber and a co-vulcanizing agent for NBR/PVC blended elastomer. Mixing compound containing TCY-70 is easy to scorch, so the mixing temperature should not be too high or the mixing time should be as short as possible, and the mixing time should not be too long, the compound is stored at a lower temperature; however, in order to improve the storage stability of the compound containing TCY-70, a pre-dispersed scorch retarder CTP-80 can be added to the formulation; in addition, TCY-70 has a tendency to increase the bond strength of rubber to metal.

Product Description

pre-dispersed crosslinking agentTCY-70

 

Product Features

active ingredient

2,4, 6-Trimercapto-s-triazine (TCY)

active content

70%

Carrier type

Ethereal rubber (ECO)

Appearance (visual inspection)

yellow particles

Density

~1.49g/cm(20 ℃)

 

Product characteristicsUnder normal circumstances, the pre-dispersed crosslinking agent TCY-70 can be used as an effective vulcanizing agent for halogen-containing rubber, such as CO, ECO, CIIR and BIIR, as well as a vulcanizing agent for ACM rubber and a co-vulcanizing agent for NBR/PVC blended elastomer. Mixing compound containing TCY-70 is easy to scorch, so the mixing temperature should not be too high or the mixing time should be as short as possible, and the mixing time should not be too long, the compound is stored at a lower temperature; however, in order to improve the storage stability of the compound containing TCY-70, a pre-dispersed scorch retarder CTP-80 can be added to the formulation; in addition, TCY-70 has a tendency to increase the bond strength of rubber to metal.

Processing characteristicsPowder TCY raw materials in the mixing process, it is difficult to disperse evenly;

It is dispersed in various halogen-containing rubbers, which greatly improves the activity of TCY.

Dosage

Mixing rubber

vulcanization system

ACM, parts

CO/ECO,份

CIIR/BIIR,

TCY-70

0.7~2.1

0.7~1.4

1.4~2.9

ZDBC-80

0.6~1.9

CTP-80 

0~1.2

0~1.2

MgO-75

4.0

0.4~0.7

 

ApplicationUsed for CO, ECO, ACM, CIIR, BIIR and other rubber products; NBR/PVC blend compound co-crosslinking agent.

PackagingComposite paper bag, lined with plastic film bag, net weight 20kg.

StorageSealed and stored in a cool, dry, well-ventilated place, avoid direct sunlight, and can be stored for 1 year.

Safety and toxicityPlease refer to the relevant product safety data (MSDS).